Injection molding
In the injection molding industry, categorizing plastics simply as "crystalline" and "amorphous" is the starting point for understanding all process parameters (especially mold temperature, cooling, and shrinkage). Many products fail to mold properly not because the machine operator lacks skill, but because the parameters aren't set in accordance with the physical nature of the material.
Injection Molding Materials - hainamould Mould Company Limted
1. What Exactly Is "Crystallinity"?
Strictly speaking, the "crystalline plastics" commonly used in injection molding (such as PP, PE, PA, POM, and PBT) are actually semi-crystalline. During cooling, a portion of their molecular chains folds and arranges in an orderly manner, forming a dense "crystalline region"; the other portion remains disordered, forming an "amorphous region."
In contrast, "amorphous plastics" (such as ABS, PC, PS, PVC, and PMMA) have molecular chains that are always in random disarray, like a tangled mess.
This difference in microstructure directly leads to completely different sensitivities to injection molding processes.
2. Core Differences in Injection Molding Performance
i. Shrinkage: Do They "Take Their Cues from Mold Temperature"?
Crystalline plastics: Shrinkage is very high (typically 1.5% – 2.5% or even more) and extremely dependent on mold temperature. The higher the mold temperature, the more time and energy the molecular chains have to arrange themselves (crystallize); the higher the crystallinity, the greater the volumetric shrinkage. If mold temperature is unstable, dimensions simply cannot be controlled.
Amorphous plastics: Shrinkage is low (typically 0.4% – 0.8%) and less sensitive to mold temperature. Dimensional changes depend mainly on thermal expansion and contraction, not on internal structural reorganization.
ii. Cooling Process: Do They "Release Latent Heat"?
Crystalline plastics: During cooling and solidification, the crystallization process releases latent heat. This means their cooling rate is slower than one might expect, and they often require longer cooling times to prevent deformation or ejector pin push-through after ejection.
Amorphous plastics: There is no latent heat of crystallization; cooling is purely heat conduction. As long as the temperature drops below the glass transition temperature (Tg), the part becomes rigid enough to demold, so cooling times are relatively short.
iii. Surface Appearance: Transparency and Gloss
Crystalline plastics: Because of the crystalline regions, light cannot pass through completely, so they are typically opaque or translucent (like PP and PE). Achieving a high-gloss surface requires very high mold temperatures to refine the surface crystallization.
Amorphous plastics: With disordered molecular arrangement, light can pass through, so most are transparent (like PC, PMMA, and PS).
3. Practical Strategies for Process Adjustment
For crystalline plastics (PP, PA, POM, etc.):
·Mold temperature is key: Don't blindly lower mold temperature to save time. It affects not only appearance but also final dimensions. You must use chillers or mold temperature controllers to tightly control the overall temperature and the temperature difference between the moving and fixed halves.
·Provide sufficient holding pressure: Because shrinkage is high, holding pressure and time must be sufficient until the gate completely freezes, to compensate for shrinkage at thick walls.
·Accept their opacity: If the product requires transparency, only amorphous materials can be used.
For amorphous plastics (ABS, PC, etc.):
·Watch for internal stress: Although dimensions are easier to control, amorphous plastics (especially PC) are extremely sensitive to shear stress. Injection speed should not be too fast, and holding pressure should not be too high, otherwise stress cracking is likely.
·Make full use of high fluidity: Amorphous plastics generally require higher injection temperatures and higher mold temperatures (e.g., PC mold temperatures can reach 80–100°C) to ensure filling.
·Prevent mold sticking: Amorphous materials tend to "stick" after solidification, so draft angles must be sufficient and the ejection mechanism must be properly designed.
Summary
When selecting materials: for low shrinkage, stable dimensions, and transparency, choose amorphous; for chemical resistance, high toughness, and wear resistance, choose crystalline (semi-crystalline).
When adjusting processes: With crystalline plastics, your core opponents are "shrinkage" and "crystallinity"; with amorphous plastics, your core opponents are "fluidity" and "internal stress." Adjust parameters in accordance with the material's nature, and the scrap rate will naturally come down.